tech / sci.engr.joining.welding / Re: Lincoln wire-matic 255 feed/speed problem

SubjectAuthor
o Lincoln wire-matic 255 feed/speed problemHaroldharley1962

1
Re: Lincoln wire-matic 255 feed/speed problem

<171aaafe4f9069aa$1$118205$4256dc03@news.newsgroupdirect.com>

  copy mid

http://novabbs.i2p/tech/article-flat.php?id=841&group=sci.engr.joining.welding#841

  copy link   Newsgroups: rec.crafts.metalworking sci.engr.joining.welding
From: 856204f47e4ba74e35b54b723294b9b3@example.com (Haroldharley1962)
Newsgroups: rec.crafts.metalworking,sci.engr.joining.welding
Subject: Re: Lincoln wire-matic 255 feed/speed problem
X-poster: Hermes 2.0
References: <1Yudnbr65_52bE7PnZ2dnUVZ_radnZ2d@giganews.com>
In-Reply-To: <1Yudnbr65_52bE7PnZ2dnUVZ_radnZ2d@giganews.com>
Content-Transfer-Encoding: 8bit
Injection-Info: 6b4fc0d3e453ddd24dc657c7b551cb88;85ed1081d970d652ce4b0362ded5a6ca
Content-Type: text/plain; charset="iso-8859-1"; format="flowed"
Lines: 5
Path: i2pn2.org!i2pn.org!usenet.blueworldhosting.com!feed1.usenet.blueworldhosting.com!peer02.iad!feed-me.highwinds-media.com!news.highwinds-media.com!feeder.usenetexpress.com!tr2.iad1.usenetexpress.com!news.newsgroupdirect.com!not-for-mail
Date: Mon, 03 Oct 2022 21:03:41 +0000
NNTP-Posting-Date: Mon, 03 Oct 2022 21:03:41 +0000
Organization: NewsgroupDirect
X-Complaints-To: abuse@newsgroupdirect.com
Message-ID: <171aaafe4f9069aa$1$118205$4256dc03@news.newsgroupdirect.com>
X-Received-Bytes: 1187
 by: Haroldharley1962 - Mon, 3 Oct 2022 21:03 UTC

Turn the welder off hold the trigger on turn the wire speed clear full all the way then to power up it will beep three times that will be fast start instead of slow start

--
For full context, visit https://www.polytechforum.com/welding/lincoln-wire-matic-255-feed-speed-problem-52609-.htm